Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (0) You Searched For: capacity-for-being-cold-worked:"Fair" elongation:[33 TO 36] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C46400 Naval Brass, Uninhibited Yes C46400 Profile Suppliers of C46400 C46500 Naval Brass, Arsenical Yes C46500 Profile Suppliers of C46500 C46600 Tin Brass No C46600 Profile Suppliers of C46600 C46700 Tin Brass No C46700 Profile Suppliers of C46700 C48640 Yes C48640 Profile Suppliers of C48640 C85570 Yes C85570 Profile Suppliers of C85570 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>