Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (0) You Searched For: capacity-for-being-cold-worked:"Poor" modulus-of-elasticity-in-tension:[14000 TO 15000] modulus-of-elasticity-in-tension:[15000 TO 16000] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C37700 Forging Brass Yes C37700 Profile Suppliers of C37700 C48200 Naval Brass, Medium Leaded Yes C48200 Profile Suppliers of C48200 C48500 Naval Brass, High Leaded Yes C48500 Profile Suppliers of C48500 C67500 Manganese Bronze A Yes C67500 Profile Suppliers of C67500 C67600 Yes C67600 Profile Suppliers of C67600 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>