10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C46400 |
Naval Brass, Uninhibited | Yes |
C46400 Profile Suppliers of C46400 |
C46500 |
Naval Brass, Arsenical | Yes |
C46500 Profile Suppliers of C46500 |
C46600 |
Tin Brass | No |
C46600 Profile Suppliers of C46600 |
C46700 |
Tin Brass | No |
C46700 Profile Suppliers of C46700 |
C65500 * |
High-Silicon Bronze A | Yes |
C65500 Profile Suppliers of C65500 |
C66430 * |
Yes |
C66430 Profile Suppliers of C66430 |
|
C69300 * |
ECO Brass | Yes |
C69300 Profile Suppliers of C69300 |
C69310 * |
SnEco | Yes |
C69310 Profile Suppliers of C69310 |
C87850 * |
Copper Silicon Alloy | Yes |
C87850 Profile Suppliers of C87850 |
C87860 * |
Yes |
C87860 Profile Suppliers of C87860 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |