Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (7) You Searched For: capacity-for-being-hot-formed:"Excellent" modulus-of-elasticity-in-tension:[19000 TO 20000] electrical-conductivity:[40.0 TO 45.0] CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C17450 * Copper Beryllium Yes C17450 Profile Suppliers of C17450 C17460 * Copper Beryllium Yes C17460 Profile Suppliers of C17460 C64750 * Yes C64750 Profile Suppliers of C64750 C70260 * Yes C70260 Profile Suppliers of C70260 C70265 * Yes C70265 Profile Suppliers of C70265 C70270 * Yes C70270 Profile Suppliers of C70270 C70315 STOL 94 Yes C70315 Profile Suppliers of C70315 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>