Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (32) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (12) You Searched For: capacity-for-being-hot-formed:"Excellent" spot-weld:"Good" soldering:"Excellent" CLEAR this search X SAVE this search << Page 1 >> 34 Alloys Found Alloy UNS#DesignationActiveView C15500 * Yes C15500 Profile Suppliers of C15500 C18145 Yes C18145 Profile Suppliers of C18145 C27450 Yellow Brass Yes C27450 Profile Suppliers of C27450 C27451 Yellow Brass (Yellow Brass) Yes C27451 Profile Suppliers of C27451 C27460 Yes C27460 Profile Suppliers of C27460 C28000 * Muntz Metal, 60% Yes C28000 Profile Suppliers of C28000 C28340 Yes C28340 Profile Suppliers of C28340 C28500 Copper-Zinc- Alloy (Brass) Yes C28500 Profile Suppliers of C28500 C28550 Yes C28550 Profile Suppliers of C28550 C46400 Naval Brass, Uninhibited Yes C46400 Profile Suppliers of C46400 C46500 Naval Brass, Arsenical Yes C46500 Profile Suppliers of C46500 C46600 Tin Brass No C46600 Profile Suppliers of C46600 C46700 Tin Brass No C46700 Profile Suppliers of C46700 C49355 * Copper Zinc Bismuth Alloy Yes C49355 Profile Suppliers of C49355 C50590 * Yes C50590 Profile Suppliers of C50590 C50705 * Yes C50705 Profile Suppliers of C50705 C64760 * Yes C64760 Profile Suppliers of C64760 C67500 Manganese Bronze A Yes C67500 Profile Suppliers of C67500 C67600 Yes C67600 Profile Suppliers of C67600 C68370 Yes C68370 Profile Suppliers of C68370 C69230 * Yes C69230 Profile Suppliers of C69230 C69240 Yes C69240 Profile Suppliers of C69240 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69310 * SnEco Yes C69310 Profile Suppliers of C69310 C69350 Yes C69350 Profile Suppliers of C69350 C69400 Silicon Red Brass Yes C69400 Profile Suppliers of C69400 C69410 Yes C69410 Profile Suppliers of C69410 C69430 Yes C69430 Profile Suppliers of C69430 C69750 Yes C69750 Profile Suppliers of C69750 C69850 Yes C69850 Profile Suppliers of C69850 C87850 * Copper Silicon Alloy Yes C87850 Profile Suppliers of C87850 C87860 * Yes C87860 Profile Suppliers of C87860 C87870 * Yes C87870 Profile Suppliers of C87870 C89841 Copper-Bismuth Alloy Yes C89841 Profile Suppliers of C89841 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>