Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (31) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (14) You Searched For: capacity-for-being-hot-formed:"Excellent" tensile-strength:[70 TO 80] element_names:"Silicon" CLEAR this search X SAVE this search << Page 1 >> 31 Alloys Found Alloy UNS#DesignationActiveView C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C18060 Yes C18060 Profile Suppliers of C18060 C18080 Yes C18080 Profile Suppliers of C18080 C46270 Yes C46270 Profile Suppliers of C46270 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C64200 * Aluminum Bronze Yes C64200 Profile Suppliers of C64200 C64740 * Yes C64740 Profile Suppliers of C64740 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C65400 Yes C65400 Profile Suppliers of C65400 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C66710 Yes C66710 Profile Suppliers of C66710 C66907 Yes C66907 Profile Suppliers of C66907 C67340 Yes C67340 Profile Suppliers of C67340 C67400 Yes C67400 Profile Suppliers of C67400 C68300 * Copper-Znc Alloy (Silicon Modified Brass) Yes C68300 Profile Suppliers of C68300 C68370 Yes C68370 Profile Suppliers of C68370 C68400 * Yes C68400 Profile Suppliers of C68400 C69150 * Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile Suppliers of C69150 C69240 Yes C69240 Profile Suppliers of C69240 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69310 * SnEco Yes C69310 Profile Suppliers of C69310 C69350 Yes C69350 Profile Suppliers of C69350 C69400 Silicon Red Brass Yes C69400 Profile Suppliers of C69400 C69410 Yes C69410 Profile Suppliers of C69410 C69430 Yes C69430 Profile Suppliers of C69430 C69710 Yes C69710 Profile Suppliers of C69710 C69850 Yes C69850 Profile Suppliers of C69850 C70260 * Yes C70260 Profile Suppliers of C70260 C70270 * Yes C70270 Profile Suppliers of C70270 C70315 STOL 94 Yes C70315 Profile Suppliers of C70315 C87860 * Yes C87860 Profile Suppliers of C87860 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>