Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (9) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (7) You Searched For: capacity-for-being-hot-formed:"Excellent" tensile-strength:[90 TO 100] density:[0.31 TO 0.32] CLEAR this search X SAVE this search << Page 1 >> 10 Alloys Found Alloy UNS#DesignationActiveView C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C40950 * Yes C40950 Profile Suppliers of C40950 C64740 * Yes C64740 Profile Suppliers of C64740 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C66430 * Yes C66430 Profile Suppliers of C66430 C70260 * Yes C70260 Profile Suppliers of C70260 C70270 * Yes C70270 Profile Suppliers of C70270 C70315 STOL 94 Yes C70315 Profile Suppliers of C70315 C72670 Yes C72670 Profile Suppliers of C72670 C79360 Yes C79360 Profile Suppliers of C79360 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>