Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (0) You Searched For: casting-yield:"High" soldering:"Good" gassing:"Medium" CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C89325 Yes C89325 Profile Suppliers of C89325 C93400 Yes C93400 Profile Suppliers of C93400 C93600 Yes C93600 Profile Suppliers of C93600 C93800 Anti-acid Metal Yes C93800 Profile Suppliers of C93800 C93900 79-6-15 Yes C93900 Profile Suppliers of C93900 C94300 Soft Bronze Yes C94300 Profile Suppliers of C94300 C94500 Yes C94500 Profile Suppliers of C94500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>