Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C17410 * |
Copper Beryllium | Yes |
C17410 Profile Suppliers of C17410 |
C17500 * |
Copper Beryllium | Yes |
C17500 Profile Suppliers of C17500 |
C17510 * |
Copper Beryllium | Yes |
C17510 Profile Suppliers of C17510 |
C51080 * |
Yes |
C51080 Profile Suppliers of C51080 |
|
C51180 * |
Yes |
C51180 Profile Suppliers of C51180 |
|
C52100 * |
Phospher Bronze, 8% C | Yes |
C52100 Profile Suppliers of C52100 |
C64400 * |
Aluminum Bronze | No |
C64400 Profile Suppliers of C64400 |
C65400 |
Yes |
C65400 Profile Suppliers of C65400 |
|
C65500 * |
High-Silicon Bronze A | Yes |
C65500 Profile Suppliers of C65500 |
C82500 * |
Copper Beryllium 20C | Yes |
C82500 Profile Suppliers of C82500 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |