Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (1) You Searched For: coated-metal-arc-welding:"Not Recommended" capacity-for-being-hot-formed:"Fair" melting-point-liquidus:[1600 TO 1700] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C27400 * Yellow Brass, 63% Yes C27400 Profile Suppliers of C27400 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>