Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (0) You Searched For: coated-metal-arc-welding:"Not Recommended" density:[0.29 TO 0.3] brazing:"Good" CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C27250 Yes C27250 Profile Suppliers of C27250 C27550 Yes C27550 Profile Suppliers of C27550 C67400 Yes C67400 Profile Suppliers of C67400 C67420 Yes C67420 Profile Suppliers of C67420 C99750 Yes C99750 Profile Suppliers of C99750 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>