Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
13 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C10100 * |
Oxygen-Free-Electronic (OFE) | Yes |
C10100 Profile Suppliers of C10100 |
C18400 |
Chromium Copper | Yes |
C18400 Profile Suppliers of C18400 |
C26100 * |
Brass | No |
C26100 Profile Suppliers of C26100 |
C26130 * |
Yes |
C26130 Profile Suppliers of C26130 |
|
C27453 |
Copper Zinc Alloy | Yes |
C27453 Profile Suppliers of C27453 |
C28340 |
Yes |
C28340 Profile Suppliers of C28340 |
|
C36600 |
Leaded Muntz Metal, Arsinical | No |
C36600 Profile Suppliers of C36600 |
C44300 * |
Admiralty, Arsenical | Yes |
C44300 Profile Suppliers of C44300 |
C46500 |
Naval Brass, Arsenical | Yes |
C46500 Profile Suppliers of C46500 |
C68700 * |
Aluminum Brass, Arsenical | Yes |
C68700 Profile Suppliers of C68700 |
C85560 |
Yes |
C85560 Profile Suppliers of C85560 |
|
C85800 |
Yes |
C85800 Profile Suppliers of C85800 |
|
C87900 |
Copper Silicon | Yes |
C87900 Profile Suppliers of C87900 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |