Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (2) You Searched For: coated-metal-arc-welding:"Not Recommended" elongation:[9 TO 12] elongation:[57 TO 60] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C16210 * High Copper Alloy No C16210 Profile Suppliers of C16210 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>