Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
11 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C80300 * |
Copper Alloy | No |
C80300 Profile Suppliers of C80300 |
C80500 * |
Copper Alloy | No |
C80500 Profile Suppliers of C80500 |
C80700 * |
Copper Alloy | No |
C80700 Profile Suppliers of C80700 |
C80900 * |
Copper Alloy | No |
C80900 Profile Suppliers of C80900 |
C81100 * |
Yes |
C81100 Profile Suppliers of C81100 |
|
C89320 * |
Yes |
C89320 Profile Suppliers of C89320 |
|
C89510 * |
SeBiLOY I (EnviroBrass I) | Yes |
C89510 Profile Suppliers of C89510 |
C89520 * |
SeBiLOY II (EnviroBrass II) | Yes |
C89520 Profile Suppliers of C89520 |
C89835 * |
Federalloy III-932 | Yes |
C89835 Profile Suppliers of C89835 |
C89845 * |
Copper-Bismuth-Alloy | Yes |
C89845 Profile Suppliers of C89845 |
C89940 * |
Yes |
C89940 Profile Suppliers of C89940 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |