Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (8) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (1) You Searched For: coated-metal-arc-welding:"Not Recommended" fluidity:"Medium" casting-yield:"Medium" CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C85700 Leaded Yellow Brass Yes C85700 Profile Suppliers of C85700 C89940 * Yes C89940 Profile Suppliers of C89940 C92200 Navy M Bronze Yes C92200 Profile Suppliers of C92200 C92300 Leaded Tin Bronze Yes C92300 Profile Suppliers of C92300 C92600 Yes C92600 Profile Suppliers of C92600 C92700 Leaded Tin Bronze Yes C92700 Profile Suppliers of C92700 C92800 Yes C92800 Profile Suppliers of C92800 C94800 Yes C94800 Profile Suppliers of C94800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>