Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (1) You Searched For: coated-metal-arc-welding:"Not Recommended" fluidity:"Medium" elongation:[30 TO 33] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C83400 Yes C83400 Profile Suppliers of C83400 C89320 * Yes C89320 Profile Suppliers of C89320 C89844 Yes C89844 Profile Suppliers of C89844 C92200 Navy M Bronze Yes C92200 Profile Suppliers of C92200 C92600 Yes C92600 Profile Suppliers of C92600 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>