Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (4) U.S. EPA Registered Antimicrobial (6) You Searched For: coated-metal-arc-welding:"Not Recommended" fluidity:"Medium" melting-point-liquidus:[1900 TO 2000] CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C80300 * Copper Alloy No C80300 Profile Suppliers of C80300 C80500 * Copper Alloy No C80500 Profile Suppliers of C80500 C80700 * Copper Alloy No C80700 Profile Suppliers of C80700 C80900 * Copper Alloy No C80900 Profile Suppliers of C80900 C81100 * Yes C81100 Profile Suppliers of C81100 C81500 Chrome Copper Yes C81500 Profile Suppliers of C81500 C83400 Yes C83400 Profile Suppliers of C83400 C89320 * Yes C89320 Profile Suppliers of C89320 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>