Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (2) You Searched For: coated-metal-arc-welding:"Not Recommended" spot-weld:"Fair" oxyacetylene-welding:"Fair" CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C33000 Low Leaded Brass (Tube) Yes C33000 Profile Suppliers of C33000 C33100 Leaded Brass No C33100 Profile Suppliers of C33100 C33200 High Leaded Brass (Tube) Yes C33200 Profile Suppliers of C33200 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C36300 Copper-Zinc-Lead Alloy Yes C36300 Profile Suppliers of C36300 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41120 * Yes C41120 Profile Suppliers of C41120 C46750 Yes C46750 Profile Suppliers of C46750 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>