Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: coated-metal-arc-welding:"Not Recommended" tensile-strength:[100 TO 110] melting-point-liquidus:[2000 TO 2100] CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C81540 Yes C81540 Profile Suppliers of C81540 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>