Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (35) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (8) You Searched For: coated-metal-arc-welding:"Not Recommended" element_names:"Sulfur" CLEAR this search X SAVE this search << Page 1 >> 37 Alloys Found Alloy UNS#DesignationActiveView C14700 * Sulfur-Bearing Yes C14700 Profile Suppliers of C14700 C14710 * Copper Alloy No C14710 Profile Suppliers of C14710 C14720 Copper Alloy No C14720 Profile Suppliers of C14720 C83400 Yes C83400 Profile Suppliers of C83400 C83450 Yes C83450 Profile Suppliers of C83450 C85200 Leaded Yellow Brass Yes C85200 Profile Suppliers of C85200 C85800 Yes C85800 Profile Suppliers of C85800 C87900 Copper Silicon Yes C87900 Profile Suppliers of C87900 C89320 * Yes C89320 Profile Suppliers of C89320 C89325 Yes C89325 Profile Suppliers of C89325 C89510 * SeBiLOY I (EnviroBrass I) Yes C89510 Profile Suppliers of C89510 C89520 * SeBiLOY II (EnviroBrass II) Yes C89520 Profile Suppliers of C89520 C89835 * Federalloy III-932 Yes C89835 Profile Suppliers of C89835 C89844 Yes C89844 Profile Suppliers of C89844 C89940 * Yes C89940 Profile Suppliers of C89940 C90280 * Yes C90280 Profile Suppliers of C90280 C92200 Navy M Bronze Yes C92200 Profile Suppliers of C92200 C92300 Leaded Tin Bronze Yes C92300 Profile Suppliers of C92300 C92500 Yes C92500 Profile Suppliers of C92500 C92600 Yes C92600 Profile Suppliers of C92600 C92700 Leaded Tin Bronze Yes C92700 Profile Suppliers of C92700 C92800 Yes C92800 Profile Suppliers of C92800 C92900 Yes C92900 Profile Suppliers of C92900 C93200 Yes C93200 Profile Suppliers of C93200 C93400 Yes C93400 Profile Suppliers of C93400 C93500 Yes C93500 Profile Suppliers of C93500 C93600 Yes C93600 Profile Suppliers of C93600 C93700 Bearing Bronze Yes C93700 Profile Suppliers of C93700 C93800 Anti-acid Metal Yes C93800 Profile Suppliers of C93800 C93900 79-6-15 Yes C93900 Profile Suppliers of C93900 C94300 Soft Bronze Yes C94300 Profile Suppliers of C94300 C94400 Yes C94400 Profile Suppliers of C94400 C94500 Yes C94500 Profile Suppliers of C94500 C94800 Yes C94800 Profile Suppliers of C94800 C97300 Yes C97300 Profile Suppliers of C97300 C97600 Yes C97600 Profile Suppliers of C97600 C97800 Yes C97800 Profile Suppliers of C97800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>