Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: density:[0.29 TO 0.3] capacity-for-being-hot-formed:"Excellent" element_names:"Zirconium" CLEAR this search X SAVE this search << Page 1 >> 2 Alloys Found Alloy UNS#DesignationActiveView C87860 * Yes C87860 Profile Suppliers of C87860 C87870 * Yes C87870 Profile Suppliers of C87870 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>