Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: density:[0.29 TO 0.3] coated-metal-arc-welding:"Fair" melting-point-solidus:[1600 TO 1650] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C79860 Yes C79860 Profile Suppliers of C79860 C82400 * Copper Beryllium 165C Yes C82400 Profile Suppliers of C82400 C82800 * Copper Beryllium 275C Yes C82800 Profile Suppliers of C82800 C86350 * Manganese Bronze Alloy Yes C86350 Profile Suppliers of C86350 C89580 * Yes C89580 Profile Suppliers of C89580 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>