Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (2) You Searched For: density:[0.29 TO 0.3] element_names:"Silicon" capacity-for-being-hot-formed:"Good" CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C27550 Yes C27550 Profile Suppliers of C27550 C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C79860 Yes C79860 Profile Suppliers of C79860 C87845 * Copper-Silicon-Brass Yes C87845 Profile Suppliers of C87845 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>