Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (21) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (15) You Searched For: density:[0.29 TO 0.3] rockwell-b-scale:[80 TO 90] element_names:"Copper" CLEAR this search X SAVE this search << Page 1 >> 23 Alloys Found Alloy UNS#DesignationActiveView C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C49355 * Copper Zinc Bismuth Alloy Yes C49355 Profile Suppliers of C49355 C63800 * Yes C63800 Profile Suppliers of C63800 C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C66900 * Manganese Brass Yes C66900 Profile Suppliers of C66900 C67300 Yes C67300 Profile Suppliers of C67300 C67400 Yes C67400 Profile Suppliers of C67400 C67420 Yes C67420 Profile Suppliers of C67420 C68800 * Yes C68800 Profile Suppliers of C68800 C69000 * Copper Zinc No C69000 Profile Suppliers of C69000 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69310 * SnEco Yes C69310 Profile Suppliers of C69310 C69400 Silicon Red Brass Yes C69400 Profile Suppliers of C69400 C69410 Yes C69410 Profile Suppliers of C69410 C69710 Yes C69710 Profile Suppliers of C69710 C69850 Yes C69850 Profile Suppliers of C69850 C82500 * Copper Beryllium 20C Yes C82500 Profile Suppliers of C82500 C82600 * Copper Beryllium 245C Yes C82600 Profile Suppliers of C82600 C82800 * Copper Beryllium 275C Yes C82800 Profile Suppliers of C82800 C85450 * Copper Zinc Alloy Yes C85450 Profile Suppliers of C85450 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 C89720 * Copper-Bismuth Alloy (TECO) Yes C89720 Profile Suppliers of C89720 C99750 Yes C99750 Profile Suppliers of C99750 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>