Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: density:[0.31 TO 0.32] casting-yield:"High" melting-point-solidus:[1550 TO 1600] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C83600 Ounce Metal Yes C83600 Profile Suppliers of C83600 C83800 Hydraulic Bronze Yes C83800 Profile Suppliers of C83800 C89844 Yes C89844 Profile Suppliers of C89844 C90400 * Tin Bronze Yes C90400 Profile Suppliers of C90400 C90410 * Tin Bronze Yes C90410 Profile Suppliers of C90410 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>