Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (7) You Searched For: density:[0.31 TO 0.32] electrical-conductivity:[35.0 TO 40.0] elongation:[24 TO 27] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C41120 * Yes C41120 Profile Suppliers of C41120 C42220 * Yes C42220 Profile Suppliers of C42220 C50780 * Yes C50780 Profile Suppliers of C50780 C66420 * Yes C66420 Profile Suppliers of C66420 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>