Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: density:[0.31 TO 0.32] element_names:"Bismuth" modulus-of-elasticity-in-tension:[14000 TO 15000] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C28340 Yes C28340 Profile Suppliers of C28340 C49340 * GEM Brass Yes C49340 Profile Suppliers of C49340 C49345 Low Leaded GEM Brass Yes C49345 Profile Suppliers of C49345 C49350 * Bismuth Brass Alloy Yes C49350 Profile Suppliers of C49350 C84100 Yes C84100 Profile Suppliers of C84100 C89838 Yes C89838 Profile Suppliers of C89838 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>