Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (33) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (25) You Searched For: density:[0.31 TO 0.32] elongation:[0 TO 3] tensile-strength:[100 TO 110] CLEAR this search X SAVE this search << Page 1 >> 33 Alloys Found Alloy UNS#DesignationActiveView C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C19140 Yes C19140 Profile Suppliers of C19140 C19160 Yes C19160 Profile Suppliers of C19160 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C42520 * Yes C42520 Profile Suppliers of C42520 C42600 * Yes C42600 Profile Suppliers of C42600 C50710 * MF202 Yes C50710 Profile Suppliers of C50710 C50715 * Yes C50715 Profile Suppliers of C50715 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51080 * Yes C51080 Profile Suppliers of C51080 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C51900 * Yes C51900 Profile Suppliers of C51900 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52180 * Yes C52180 Profile Suppliers of C52180 C52400 * Phospher Bronze 10% D Yes C52400 Profile Suppliers of C52400 C52480 * Yes C52480 Profile Suppliers of C52480 C64725 * Copper Silicon Alloy Yes C64725 Profile Suppliers of C64725 C64751 Yes C64751 Profile Suppliers of C64751 C64770 * Yes C64770 Profile Suppliers of C64770 C66300 * Yes C66300 Profile Suppliers of C66300 C69750 Yes C69750 Profile Suppliers of C69750 C70330 Yes C70330 Profile Suppliers of C70330 C70350 * Yes C70350 Profile Suppliers of C70350 C70370 * Yes C70370 Profile Suppliers of C70370 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C76200 Nickel Silver Yes C76200 Profile Suppliers of C76200 C77000 Nickel Silver, 55-18 Yes C77000 Profile Suppliers of C77000 C79360 Yes C79360 Profile Suppliers of C79360 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>