You Searched For:
11 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C83600 |
Ounce Metal | Yes |
C83600 Profile Suppliers of C83600 |
C83800 |
Hydraulic Bronze | Yes |
C83800 Profile Suppliers of C83800 |
C84030 * |
Low Lead Semi-Red Brass | Yes |
C84030 Profile Suppliers of C84030 |
C84400 |
Valve Metal | Yes |
C84400 Profile Suppliers of C84400 |
C84800 |
Plumbing Goods Brass | Yes |
C84800 Profile Suppliers of C84800 |
C89320 * |
Yes |
C89320 Profile Suppliers of C89320 |
|
C89838 |
Yes |
C89838 Profile Suppliers of C89838 |
|
C89845 * |
Copper-Bismuth-Alloy | Yes |
C89845 Profile Suppliers of C89845 |
C90410 * |
Tin Bronze | Yes |
C90410 Profile Suppliers of C90410 |
C90420 * |
Tin Bronze | Yes |
C90420 Profile Suppliers of C90420 |
C94400 |
Yes |
C94400 Profile Suppliers of C94400 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |