Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (7) You Searched For: density:[0.31 TO 0.32] elongation:[27 TO 30] capacity-for-being-hot-formed:"Good" CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C42200 * Yes C42200 Profile Suppliers of C42200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>