Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (19) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (17) You Searched For: density:[0.31 TO 0.32] elongation:[27 TO 30] tensile-strength:[80 TO 90] CLEAR this search X SAVE this search << Page 1 >> 19 Alloys Found Alloy UNS#DesignationActiveView C15715 * Dispersion Strengthened Alloy Yes C15715 Profile Suppliers of C15715 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C42200 * Yes C42200 Profile Suppliers of C42200 C43400 * Yes C43400 Profile Suppliers of C43400 C50710 * MF202 Yes C50710 Profile Suppliers of C50710 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C51900 * Yes C51900 Profile Suppliers of C51900 C51980 * Yes C51980 Profile Suppliers of C51980 C52180 * Yes C52180 Profile Suppliers of C52180 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C71950 Yes C71950 Profile Suppliers of C71950 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C82200 * Copper Beryllium 3C Yes C82200 Profile Suppliers of C82200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>