Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (20) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (16) You Searched For: density:[0.31 TO 0.32] elongation:[30 TO 33] tensile-strength:[70 TO 80] CLEAR this search X SAVE this search << Page 1 >> 20 Alloys Found Alloy UNS#DesignationActiveView C19200 * Yes C19200 Profile Suppliers of C19200 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C42200 * Yes C42200 Profile Suppliers of C42200 C50710 * MF202 Yes C50710 Profile Suppliers of C50710 C51080 * Yes C51080 Profile Suppliers of C51080 C51900 * Yes C51900 Profile Suppliers of C51900 C51980 * Yes C51980 Profile Suppliers of C51980 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52480 * Yes C52480 Profile Suppliers of C52480 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C66430 * Yes C66430 Profile Suppliers of C66430 C72670 Yes C72670 Profile Suppliers of C72670 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 C78200 Yes C78200 Profile Suppliers of C78200 C78270 Nickel Silver (Nickel Silver) Yes C78270 Profile Suppliers of C78270 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>