Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
15 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C17500 * |
Copper Beryllium | Yes |
C17500 Profile Suppliers of C17500 |
C22000 * |
Commercial Bronze, 90% | Yes |
C22000 Profile Suppliers of C22000 |
C31400 |
Leaded Commercial Bronze | Yes |
C31400 Profile Suppliers of C31400 |
C31600 |
Leaded Commercial Bronze (Nickel-Bearing) | Yes |
C31600 Profile Suppliers of C31600 |
C40800 * |
Silicon Brass | No |
C40800 Profile Suppliers of C40800 |
C40810 * |
Yes |
C40810 Profile Suppliers of C40810 |
|
C40850 * |
Yes |
C40850 Profile Suppliers of C40850 |
|
C40860 * |
Yes |
C40860 Profile Suppliers of C40860 |
|
C41100 * |
Tin Brass | Yes |
C41100 Profile Suppliers of C41100 |
C41300 * |
Tin Brass | Yes |
C41300 Profile Suppliers of C41300 |
C41500 * |
Tin Brass | Yes |
C41500 Profile Suppliers of C41500 |
C42200 * |
Yes |
C42200 Profile Suppliers of C42200 |
|
C42520 * |
Yes |
C42520 Profile Suppliers of C42520 |
|
C50780 * |
Yes |
C50780 Profile Suppliers of C50780 |
|
C75400 |
Nickel Silver, 65-15 | Yes |
C75400 Profile Suppliers of C75400 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |