Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (6) You Searched For: density:[0.31 TO 0.32] gas-shielded-arc-welding:"Excellent" melting-point-solidus:[1850 TO 1900] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C18090 Yes C18090 Profile Suppliers of C18090 C40810 * Yes C40810 Profile Suppliers of C40810 C42200 * Yes C42200 Profile Suppliers of C42200 C42210 * Tin Brass Yes C42210 Profile Suppliers of C42210 C42220 * Yes C42220 Profile Suppliers of C42220 C64740 * Yes C64740 Profile Suppliers of C64740 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>