Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (8) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: density:[0.31 TO 0.32] gas-shielded-arc-welding:"Not Recommended" yield-strength:[90 TO 110] CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C15720 * Dispersion Strengthned Alloy Yes C15720 Profile Suppliers of C15720 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19140 Yes C19140 Profile Suppliers of C19140 C19160 Yes C19160 Profile Suppliers of C19160 C64770 * Yes C64770 Profile Suppliers of C64770 C64775 Copper-nickel-silicon Yes C64775 Profile Suppliers of C64775 C64790 Yes C64790 Profile Suppliers of C64790 C70240 * Yes C70240 Profile Suppliers of C70240 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>