Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (6) You Searched For: density:[0.31 TO 0.32] rockwell-30t-scale:[65 TO 70] rockwell-b-scale:[30 TO 40] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>