Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (5) You Searched For: density:[0.31 TO 0.32] rockwell-b-scale:[50 TO 60] modulus-of-elasticity-in-tension:[15000 TO 16000] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52400 * Phospher Bronze 10% D Yes C52400 Profile Suppliers of C52400 C81800 * Copper Beryllium 50C No C81800 Profile Suppliers of C81800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>