Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: density:[0.31 TO 0.32] soldering:"Excellent" element_names:"Selenium" CLEAR this search X SAVE this search << Page 1 >> 2 Alloys Found Alloy UNS#DesignationActiveView C42210 * Tin Brass Yes C42210 Profile Suppliers of C42210 C89510 * SeBiLOY I (EnviroBrass I) Yes C89510 Profile Suppliers of C89510 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>