Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (1) You Searched For: density:[0.31 TO 0.32] tensile-strength:[100 TO 110] density:[0.3 TO 0.31] CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C44250 * Yes C44250 Profile Suppliers of C44250 C44710 Yes C44710 Profile Suppliers of C44710 C76200 Nickel Silver Yes C76200 Profile Suppliers of C76200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>