10 Alloys Found

Alloy UNS#DesignationActiveView

C84030 *

Low Lead Semi-Red Brass Yes C84030 Profile
Suppliers of C84030

C84200

Yes C84200 Profile
Suppliers of C84200

C84500

Yes C84500 Profile
Suppliers of C84500

C90300

Tin Bronze Yes C90300 Profile
Suppliers of C90300

C90500

Gun Metal Yes C90500 Profile
Suppliers of C90500

C90700

Tin Bronze, 65 Yes C90700 Profile
Suppliers of C90700

C92200

Navy M Bronze Yes C92200 Profile
Suppliers of C92200

C92300

Leaded Tin Bronze Yes C92300 Profile
Suppliers of C92300

C92600

Yes C92600 Profile
Suppliers of C92600

C92900

Yes C92900 Profile
Suppliers of C92900