Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (10) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (9) You Searched For: electrical-conductivity:[10.0 TO 15.0] elongation:[33 TO 36] CLEAR this search X SAVE this search << Page 1 >> 10 Alloys Found Alloy UNS#DesignationActiveView C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C61300 * Yes C61300 Profile Suppliers of C61300 C61400 * Yes C61400 Profile Suppliers of C61400 C61500 * Yes C61500 Profile Suppliers of C61500 C62300 * Aluminum Bronze, 9% Yes C62300 Profile Suppliers of C62300 C63800 * Yes C63800 Profile Suppliers of C63800 C72500 * Yes C72500 Profile Suppliers of C72500 C94700 * Cast Nickel-Tin Bronze Yes C94700 Profile Suppliers of C94700 C94800 Yes C94800 Profile Suppliers of C94800 C95200 * Yes C95200 Profile Suppliers of C95200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>