Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: electrical-conductivity:[5.0 TO 10.0] modulus-of-elasticity-in-tension:[19000 TO 20000] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C19950 Yes C19950 Profile Suppliers of C19950 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C72200 Yes C72200 Profile Suppliers of C72200 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 C96300 * Yes C96300 Profile Suppliers of C96300 C97600 Yes C97600 Profile Suppliers of C97600 C99500 * Special Alloys Yes C99500 Profile Suppliers of C99500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>