Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
15 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C12200 * |
Phosphorus-Deoxidized, High Residual P (DHP) | Yes |
C12200 Profile Suppliers of C12200 |
C12210 * |
Yes |
C12210 Profile Suppliers of C12210 |
|
C14310 * |
Cadmium Copper | No |
C14310 Profile Suppliers of C14310 |
C18080 |
Yes |
C18080 Profile Suppliers of C18080 |
|
C18100 |
Yes |
C18100 Profile Suppliers of C18100 |
|
C18145 |
Yes |
C18145 Profile Suppliers of C18145 |
|
C18147 |
Yes |
C18147 Profile Suppliers of C18147 |
|
C18200 |
Chromium Copper | Yes |
C18200 Profile Suppliers of C18200 |
C18400 |
Chromium Copper | Yes |
C18400 Profile Suppliers of C18400 |
C18500 |
High Copper | No |
C18500 Profile Suppliers of C18500 |
C18620 * |
Hiigh Copper | Yes |
C18620 Profile Suppliers of C18620 |
C18625 * |
HRSC | Yes |
C18625 Profile Suppliers of C18625 |
C19210 * |
Yes |
C19210 Profile Suppliers of C19210 |
|
C19217 |
Yes |
C19217 Profile Suppliers of C19217 |
|
C19720 * |
Yes |
C19720 Profile Suppliers of C19720 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |