Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: element_names:"Antimony" soldering:"Excellent" element_names:"Selenium" CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C68370 Yes C68370 Profile Suppliers of C68370 C89510 * SeBiLOY I (EnviroBrass I) Yes C89510 Profile Suppliers of C89510 C89520 * SeBiLOY II (EnviroBrass II) Yes C89520 Profile Suppliers of C89520 C89530 Copper-Bismuth-Selenium Alloy (Brasses) Yes C89530 Profile Suppliers of C89530 C89535 Copper-Bismuth Alloy Yes C89535 Profile Suppliers of C89535 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>