31 Alloys Found

Alloy UNS#DesignationActiveView

C10100 *

Oxygen-Free-Electronic (OFE) Yes C10100 Profile
Suppliers of C10100

C11025 *

Fire Refined High Conductivity (FRHC) Yes C11025 Profile
Suppliers of C11025

C11040 *

Yes C11040 Profile
Suppliers of C11040

C11045 *

ETP (ETP) Yes C11045 Profile
Suppliers of C11045

C12500 *

Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile
Suppliers of C12500

C12900 *

Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile
Suppliers of C12900

C14200 *

Phosphorus-Deoxidized, Arsenical (DPA) Yes C14200 Profile
Suppliers of C14200

C18400

Chromium Copper Yes C18400 Profile
Suppliers of C18400

C26130 *

Yes C26130 Profile
Suppliers of C26130

C27453

Copper Zinc Alloy Yes C27453 Profile
Suppliers of C27453

C28340

Yes C28340 Profile
Suppliers of C28340

C35330

DZR Brass Yes C35330 Profile
Suppliers of C35330

C44300 *

Admiralty, Arsenical Yes C44300 Profile
Suppliers of C44300

C46500

Naval Brass, Arsenical Yes C46500 Profile
Suppliers of C46500

C48600

DZR Brass Yes C48600 Profile
Suppliers of C48600

C60800

Yes C60800 Profile
Suppliers of C60800

C63400 *

Aluminum Bronze Yes C63400 Profile
Suppliers of C63400

C63600

Yes C63600 Profile
Suppliers of C63600

C64200 *

Aluminum Bronze Yes C64200 Profile
Suppliers of C64200

C64210 *

Aluminum Silicon Bronze Yes C64210 Profile
Suppliers of C64210

C68320

Yes C68320 Profile
Suppliers of C68320

C68700 *

Aluminum Brass, Arsenical Yes C68700 Profile
Suppliers of C68700

C69430

Yes C69430 Profile
Suppliers of C69430

C69710

Yes C69710 Profile
Suppliers of C69710

C85560

Yes C85560 Profile
Suppliers of C85560

C85570

Yes C85570 Profile
Suppliers of C85570

C85660

Yes C85660 Profile
Suppliers of C85660

C85800

Yes C85800 Profile
Suppliers of C85800

C87800 *

Cast Silicon Bronze Yes C87800 Profile
Suppliers of C87800

C87845 *

Copper-Silicon-Brass Yes C87845 Profile
Suppliers of C87845

C87900

Copper Silicon Yes C87900 Profile
Suppliers of C87900
* signifies an alloy registered with the U.S. EPA as Antimicrobial.