Alloy UNS# | Designation | Active | View |
---|---|---|---|
C10100 * |
Oxygen-Free-Electronic (OFE) | Yes |
C10100 Profile Suppliers of C10100 |
C11025 * |
Fire Refined High Conductivity (FRHC) | Yes |
C11025 Profile Suppliers of C11025 |
C11040 * |
Yes |
C11040 Profile Suppliers of C11040 |
|
C11045 * |
ETP (ETP) | Yes |
C11045 Profile Suppliers of C11045 |
C11050 |
ETP-R | Yes |
C11050 Profile Suppliers of C11050 |
C12700 * |
Copper Alloy | No |
C12700 Profile Suppliers of C12700 |
C12800 * |
Copper Alloy | No |
C12800 Profile Suppliers of C12800 |
C12900 * |
Fire-Refined Tough Pitch with Ag (FRSTP) | Yes |
C12900 Profile Suppliers of C12900 |
C13000 |
Copper Alloy | No |
C13000 Profile Suppliers of C13000 |
C69900 |
Copper Zinc | No |
C69900 Profile Suppliers of C69900 |
C80300 * |
Copper Alloy | No |
C80300 Profile Suppliers of C80300 |