Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

2 Alloys Found

Alloy UNS#DesignationActiveView

C85800

Yes C85800 Profile
Suppliers of C85800

C87845 *

Copper-Silicon-Brass Yes C87845 Profile
Suppliers of C87845
* signifies an alloy registered with the U.S. EPA as Antimicrobial.