Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (4) You Searched For: element_names:"Boron" elongation:[39 TO 42] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C68410 * Yes C68410 Profile Suppliers of C68410 C80500 * Copper Alloy No C80500 Profile Suppliers of C80500 C80700 * Copper Alloy No C80700 Profile Suppliers of C80700 C84020 * Semi-Red Brass Yes C84020 Profile Suppliers of C84020 C89710 Green Brass Yes C89710 Profile Suppliers of C89710 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>