Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (2) You Searched For: element_names:"Lead" electrical-conductivity:[75.0 TO 80.0] CLEAR this search X SAVE this search << Page 1 >> 4 Alloys Found Alloy UNS#DesignationActiveView C15760 * Dispersion Strengthened Alloy Yes C15760 Profile Suppliers of C15760 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18500 High Copper No C18500 Profile Suppliers of C18500 C19720 * Yes C19720 Profile Suppliers of C19720 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>