Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C53800 |
Yes |
C53800 Profile Suppliers of C53800 |
|
C84100 |
Yes |
C84100 Profile Suppliers of C84100 |
|
C89510 * |
SeBiLOY I (EnviroBrass I) | Yes |
C89510 Profile Suppliers of C89510 |
C89535 |
Copper-Bismuth Alloy | Yes |
C89535 Profile Suppliers of C89535 |
C89833 * |
Copper Bismuth Alloy | Yes |
C89833 Profile Suppliers of C89833 |
C89837 |
Yes |
C89837 Profile Suppliers of C89837 |
|
C89838 |
Yes |
C89838 Profile Suppliers of C89838 |
|
C89845 * |
Copper-Bismuth-Alloy | Yes |
C89845 Profile Suppliers of C89845 |
C94400 |
Yes |
C94400 Profile Suppliers of C94400 |
|
C94500 |
Yes |
C94500 Profile Suppliers of C94500 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |